Grades | Base Resin |
MFI(g/10min) [1]190℃,2.16kg |
Grafting Level (MAH wt%) |
Applications | ||
GPM400A | ABS | 15-25 | ≥0.5 |
Mainly used as toughening agent for ABS/GF composites, it can improve the floating fiber phenomenon of composite materials effectively. Used as polarity regulator for ABS, it makes the material have better surface colouring, bonding and other properties. Loading dosage: 2-5% |
||
GPM450C | PPO | 20-50 | 2.9-3.1 |
Used as a compatibilizer for PPO/PA alloy. It can improve the interfacial compatibility between PPO and PA, enhance the alloy toughness and not affect the high-temperature resistance of the alloys. Loading dosage: 2-5% |
||
GPM500CY | SEBS | 0.1-1.0 | 1.0-1.3 |
A coupling agent and impact modifier for PPO cable compounds, giving good compatibility for PPO resin and filter whilst improving toughness. Highly cost-effective. |
||
GPM5601 | SEBS | 10-20 | 1.1-1.4 |
High performance SEBS modifier providing excellent performance in PA, especially for TPE over-molding elastomer. Also used as a coupling agent and impact modifier for PPO compounds, improving the compatibility of the PPO resin and filler and providing good toughness. |
||
GPM5618 | SEBS | 10-20 | 1.6-1.8 |
Cost performance SEBS modifier providing excellent performance in PA, especially for TPE over-molding elastomer. Also used as a coupling agent and impact modifier for PPO compounds, improving the compatibility of the PPO resin and filler and providing good toughness. |
||
M167 | LLDPE | 3.5-6.5 | ≥0.5 |
Used a s compatibilizer for Nylon insulation strip. it can improve the compatibility and adhesion of nylon resin with glass fiber or other non-polar fillers. Loading dosage: 5-15%. |
||
GN410 | POE/PP | 1.0-2.6 | 0.7-0.85 |
Used as compatibility and toughening agent for Heat-conducting nylon, it can improve the compatibility between nylon and glass fiber effectively and enhance the toughness of Nylon insulation strip. Loading dosage: 5-15% |
||
GPM163 | PP/mPE | 9.0-13.0 | 0.15-0.52 |
Used as compatibility and toughening agent for Heat-conducting nylon with high liquidity. It can improve the compatibility between nylon and glass fiber effectively and enhance the toughness of Nylon insulation strip. Loading dosage: 5-15%. |