Grades |
Base Resin |
MFI |
Grafting Level |
Applications |
||
FH116A | PP-H | 120-160[1] | 0.6-1.0 |
With low VOC content, end use for internal automotive parts, food and pharmaceutical packageng, providing higher strength and modulus. Recommended loading dosage 2-5% |
||
FH118A | PP-B | 100-130[1] | 0.6-1.0 |
Featuring a lower VOC content, suitable for PP-based products sensitive to small molecule residues, such as automotive interior parts, food and pharmaceutical packaging. As a typical coupling agenet used in long glass fiber reinforced PP materials, which does not yellow under high-temperature processing. Recommended loading dosage: 2-5%. |
||
FH1012 | PP-R | 70-100[1] | 0.5-1.0 |
With a lower VOC content and melting point, suitable for processes with lower processing temperatures. Typically used in encapsulation products. |
||
FH1016 | PP-R | 22-28[2] | >1.0 |
Highly active and high-melt-index maleic anhydride-modified polypropylene products, typically used in adhesive, coating, and other fields. |